Testing procedure Mechanical properties of were investigated using an Instron 5969 testing machine with the maximum load capacity 50 kN. Tension and compression tests were carried out at room temperature with the initial strain rate equal to 1 × 10-3 s-1. All specimens were cut out along ED. Flat tensile specimens, with thickness equal to 2 mm and dimensions of the gauge section 2.5 mm × 14 mm, were machined using wire electrical discharge machining (EDM).Height and diameter of the compression specimens were 8 mm and 7 mm, respectively.